Super-Solidus Hot Isostatic Pressing Heat Treatments for Advanced Single Crystal Ni-Base Superalloys

Super-solidus hot isostatic pressing (SSHIP) heat treatment has been developed and applied to CMSX-10 K, a third-generation Ni-base single crystal superalloy. This innovative approach aims to reduce the total time required for solution heat treatment while enhancing mechanical properties compared to conventional routes. SSHIP is suitable for all types of Ni-base single crystal superalloys, particularly those with high refractory element content and a significant volume fraction of eutectic microstructure in the as-cast state.

Share:

Related content

White paper

Sustainable production potential of aero engine components in alloy 718 with Flexform™

White paper

Transforming heavy manufacturing with large-scale PM-HIP

PM-AM cylinder demo part
Customer Stories

Paragon Medical elevates their medical device AM manufacturing with Quintus® Care and Quintus Purus®

Isostatic pression solutions for scalable, cost-effective solid-state battery (SSB) production
White paper

Throughput and cost analysis of solid-state battery production

Brochure

QIH 200 URC® – the largest HIP with full HPHT™ capability

White paper

Benefits of using HIP for additively manufactured thin-walled, high-performance heat exchangers