Material Densification
Technical Publication

Effects of the solution and first aging treatment applied to as-built and post-HIP CM247 produced via laser powder bed fusion (LPBF)

This work focuses on the production of CM247LC, a low weldable Ni-Based alloy, using selective laser melting (SLM). Despite initial process parameter optimization, the low defect volume fraction did not meet manufacturing standards, primarily due to the high γ’ volume fraction affecting weldability. However, a crack-free condition was achieved through a γ’-sub-solvus Hot Isostatic Pressing Cycle (HIP), reducing defects to 0.04% and stabilizing the microstructure. Further optimization of the microstructure is needed post-HIP. The paper discusses a new heat treatment recipe to enhance creep and high-temperature fatigue resistance by promoting ordered cuboidal primary γ’ precipitation. This treatment also significantly alters the crystalline structures, leading to grain coarsening and the formation of equiaxial grains.

Share:

Related content

White paper

Sustainable production potential of aero engine components in alloy 718 with Flexform™

White paper

Transforming heavy manufacturing with large-scale PM-HIP

PM-AM cylinder demo part
Customer Stories

Paragon Medical elevates their medical device AM manufacturing with Quintus® Care and Quintus Purus®

Isostatic pression solutions for scalable, cost-effective solid-state battery (SSB) production
White paper

Throughput and cost analysis of solid-state battery production

Brochure

QIH 200 URC® – the largest HIP with full HPHT™ capability

White paper

Benefits of using HIP for additively manufactured thin-walled, high-performance heat exchangers